Plastimix 250 WATER-REDUCING ADMIXTURE FOR CONCRETE DESCRIPTION: Plastimix
250 is
a ready to use aqueous solution of complex compounds which enhance the
performance of plastic and hardened concrete.
Plastimix 250 is manufactured under rigid quality control measures
to provide uniform, reliable results. USES: Plastimix
250 is
recommended for mixes where reduced water content, improved cement
performance, uniform, normal set times and enhanced finishing
characteristics are desirable. ADVANTAGES: · Improves the quality of concrete by decreasing water-cement ratio · Increases early and ultimate compressive and flexural strength ·
Reduces
cracking and shrinkage ·
Improves
workability and finishability on all flatwork, slip formed and pre-cast surfaces ·
Improves
formed surfaces while reducing segregation ·
Improves
pumpability of concrete ·
Improves
normal-setting characteristics ·
Increases
relative durability – resists damage caused by freezing and thawing ·
Improves
density and watertightness DOSAGE
RATE: Plastimix
250
is
recommended for use at a dosage rate of 3 to 5 fluid ounces per 100 pounds
(196 to 327 ml per 100 kg) of cement. Because
local job conditions vary, contact your local Pro Mix sales representative
for further assistance if using outside recommended dosage ranges. SPECIFICATIONS: Conforms
to ASTM C 494 type A AASHTO
M 194 Type A CRD
C 87 Type A TECHNICAL
NOTE: Plastimix
250
does not contain any purposely added calcium chloride or other chloride
based components. It will not
promote or contribute to corrosion of reinforcing steel in concrete. COMPATIBILITY: Plastimix
250 is
compatible with all types of Portland cement, class C and F fly ash, slag,
microsilica, calcium chloride, fibers and approved air entraining and
accelerating admixtures. Plastimix
250 can be used in all white, colored, and architectural concrete.
For best results, each admixture must be dispensed separately into
the concrete mix. STORAGE: Plastimix
250
may freeze at temperatures below 35 F (2 C).
Although freezing does not harm Plastimix 250, precautions should be taken to
protect it from freezing. If
it should happen to freeze, thaw and reconstitute with mechanical
agitations. Do Not Use Pressurized Air For Agitation. PACKAGING: 55-gallon
drums and bulk deliveries. Send mail to
Webmaster
with questions or comments about this web site. |
|
|
|
||